In recent decades zirconium oxide has been introduced in the field of dentistry as a high-strength ceramic. Unlike its mechanical advantages, however, due to its inert chemical properties, it bonds poorly to other substrates, so improving bonding strength to an adhesive material is necessary.
In this experimental study, 70 ceramic zirconia blocks were prepared and distributed randomly among 7 groups. Then the shear bond strengths were determined and the samples were examined by a scanning electron microscope (SEM). Statistical analysis was performed by one-way ANOVA and multiple Tukey comparisons.
One-way analysis of variance (ANOVA) showed that laser irradiation distance has a significant effect on orthodontics brackets bond strength to zirconia-ceramics. Based on the Tukey post hoc test, each group was compared with other groups and the contact mode and 2 mm distance groups showed significantly higher bond strength than other groups (P-value <0.05).
Orthodontic bracket bond strength to zirconia-ceramics will be reduced by increasing Er: YAG laser irradiation distance from samples. The highest bond strength will be achieved when the laser irradiation distance is 2 mm or when the laser beam is in contact with samples.
- حق عضویت دریافتی صرف حمایت از نشریات عضو و نگهداری، تکمیل و توسعه مگیران میشود.
- پرداخت حق اشتراک و دانلود مقالات اجازه بازنشر آن در سایر رسانههای چاپی و دیجیتال را به کاربر نمیدهد.