The aim of this study was the evaluation of compressive strength and setting expansion of GC and Adenta dye stones. Materials &
This study was an experimental study. The sample number was 21 for each group (n = 21). Compressive strength and setting expansion of GC and Adenta dye stones was done Based on ADA Standard 25 and Iranian Standard No. 2792. Data analysis was done with SPSS 20 software (p value = 0.05). The Independent-Sample t-test was used for data analysis.
There was no significant difference between GC (47.61 ± 5.54) and Adenta (44.31 ± 7.71) in terms of compressive strength. Also, there was no significant difference in the setting expansion between GC (0.07 ± 0.008) and adenta (0.08 ± 0.001).
Our results showed that there is no statistically significant difference in setting expansion and compressive strength between GC and Adenta dye stones and both samples was under standard condition) p value < 0.05).
- حق عضویت دریافتی صرف حمایت از نشریات عضو و نگهداری، تکمیل و توسعه مگیران میشود.
- پرداخت حق اشتراک و دانلود مقالات اجازه بازنشر آن در سایر رسانههای چاپی و دیجیتال را به کاربر نمیدهد.