Elevated Temperature Tensile Properties of Thehot Extruded Pure Aluminum Nanostructure and Al-5vol%SiC Nanocomposite

Message:
Abstract:
Al–5 vol.%SiC nanocomposite powder and pure aluminum nanostructure powder are produced by attrition milling and using pure aluminum powder with dimension of 20 to 50 µm and SiC with dimension of 20-50 nm. Then the produced powders are consolidated and strengthened by hot extrusion method. The wire cut machine was used to prepare flat tensile samples from extruded products. Tensile test were done from 25 to 300 oC. The results show that the strength of Al–5 vol. %SiC nanocomposite are higher than pure aluminum nanostructure in all temperatures. Fractography shows that the fracture of Al–5 vol. %SiC nanocomposite are brittle and pure aluminum nanostructure are ductile.
Language:
Persian
Published:
Advanced Prosesses in Materials Engineering, Volume:5 Issue: 18, 2011
Page:
57
magiran.com/p1119872  
دانلود و مطالعه متن این مقاله با یکی از روشهای زیر امکان پذیر است:
اشتراک شخصی
با عضویت و پرداخت آنلاین حق اشتراک یک‌ساله به مبلغ 1,390,000ريال می‌توانید 70 عنوان مطلب دانلود کنید!
اشتراک سازمانی
به کتابخانه دانشگاه یا محل کار خود پیشنهاد کنید تا اشتراک سازمانی این پایگاه را برای دسترسی نامحدود همه کاربران به متن مطالب تهیه نمایند!
توجه!
  • حق عضویت دریافتی صرف حمایت از نشریات عضو و نگهداری، تکمیل و توسعه مگیران می‌شود.
  • پرداخت حق اشتراک و دانلود مقالات اجازه بازنشر آن در سایر رسانه‌های چاپی و دیجیتال را به کاربر نمی‌دهد.
In order to view content subscription is required

Personal subscription
Subscribe magiran.com for 70 € euros via PayPal and download 70 articles during a year.
Organization subscription
Please contact us to subscribe your university or library for unlimited access!