Copper smelting slags are hard materials. Therefore,to recover their copper by flotation method, grinding should be carried out to obtain optimal particle size. Copper smelting slags in the Bardeskan district, with work index of 16.24 kwh/st, were grinded for 65 minutes to reach an acceptable degree of freedom for the flotation tests, with particle size of 80%, smaller than 70 μm. With this grinding time, degree of freedom for copper-bearing minerals was achieved 85-90%. The floatation method performed and the procedure used for the optimization of the effective parameters were described in this paper. The results obtained for the flotation tests, carried out at the optimal conditions after grinding the slags (with a grinding time of65 minutes), showed 62.23% of copper recovery, while, by flotation of copper slags at optimal conditions after increasing the grinding time to 85 minutes (d80 = 48µ), the Cu recovery was increased to 79.89%.
Language:
English
Published:
Journal of Mining and Environement, Volume:6 Issue: 2, Summer 2015
Pages:
237 to 249
magiran.com/p1457470  
دانلود و مطالعه متن این مقاله با یکی از روشهای زیر امکان پذیر است:
اشتراک شخصی
با عضویت و پرداخت آنلاین حق اشتراک یک‌ساله به مبلغ 1,390,000ريال می‌توانید 70 عنوان مطلب دانلود کنید!
اشتراک سازمانی
به کتابخانه دانشگاه یا محل کار خود پیشنهاد کنید تا اشتراک سازمانی این پایگاه را برای دسترسی نامحدود همه کاربران به متن مطالب تهیه نمایند!
توجه!
  • حق عضویت دریافتی صرف حمایت از نشریات عضو و نگهداری، تکمیل و توسعه مگیران می‌شود.
  • پرداخت حق اشتراک و دانلود مقالات اجازه بازنشر آن در سایر رسانه‌های چاپی و دیجیتال را به کاربر نمی‌دهد.
In order to view content subscription is required

Personal subscription
Subscribe magiran.com for 70 € euros via PayPal and download 70 articles during a year.
Organization subscription
Please contact us to subscribe your university or library for unlimited access!