Analysis of Cracks in the Pulsed Nd:YAG Laser Welded Joint of Nickel-Based Superalloy

Message:
Article Type:
Research/Original Article (دارای رتبه معتبر)
Abstract:

The weldability of GTD-111 nickel-based superalloy by pulsed Nd:YAG laser welding with an average power of 250 W was studied, and the microstructural evolution and cracking characteristics were also investigated. The solidification cracking of the fusion zone (FZ) and the intergranular liquation cracking in the heat affected zone (HAZ) were observed in the joint. Solidification cracking was caused by the residual liquid metal originated from the segregation of Ti, Nb and Al elements in the interdendritic region at the last stage of solidification. And the HAZ liquation cracking was associated with the constitutional liquation of , MC carbides, and the melting of Cr-rich boride. Ti was introduced as the most important factor in the formation of the liquation cracks in HAZ by reducing the start temperature of  eutectic reaction and increasing the dissolution temperature. Chemical analysis of the crack edges at HAZ revealed the presence of high amounts of Ti and Al elements which can be attributed to  partial melting. Gleeble physical simulation revealed that in casting the sample, the liquation started at significantly lower temperatures than in the 1200  solution heat treated samples. This is attributed to the boride and intermetallic particles, which had dissolved by the 1200  heat treatment. The formation of fine grains due to the high cooling rate of the weld as well as the formation of dispersed carbides in the fusion and heat affected zones led to an increase in the microhardness by about 130 HV compared to the base metal.

Language:
English
Published:
Iranian Journal of Materials Forming, Volume:7 Issue: 1, Winter and Spring 2020
Pages:
54 to 69
magiran.com/p2121388  
دانلود و مطالعه متن این مقاله با یکی از روشهای زیر امکان پذیر است:
اشتراک شخصی
با عضویت و پرداخت آنلاین حق اشتراک یک‌ساله به مبلغ 1,390,000ريال می‌توانید 70 عنوان مطلب دانلود کنید!
اشتراک سازمانی
به کتابخانه دانشگاه یا محل کار خود پیشنهاد کنید تا اشتراک سازمانی این پایگاه را برای دسترسی نامحدود همه کاربران به متن مطالب تهیه نمایند!
توجه!
  • حق عضویت دریافتی صرف حمایت از نشریات عضو و نگهداری، تکمیل و توسعه مگیران می‌شود.
  • پرداخت حق اشتراک و دانلود مقالات اجازه بازنشر آن در سایر رسانه‌های چاپی و دیجیتال را به کاربر نمی‌دهد.
In order to view content subscription is required

Personal subscription
Subscribe magiran.com for 70 € euros via PayPal and download 70 articles during a year.
Organization subscription
Please contact us to subscribe your university or library for unlimited access!